일반적인 플라스틱 재료 문제에 대한 실질적인 답변

1506 질문
Q
PP Injection Part Sink Mark—Freeze-off Type
A
Holding after freeze-off = ineffective feeding—the gate is the key.
Injection Molding PP;sink mark;gate freeze-off;holding pressure;thick wall
Q
PP Injection Part Metering Fluctuation
A
For unstable plasticization, check feeding first.
Injection Molding PP;plasticization fluctuation;bridging;pulverized material;feeding
Q
PP Injection Part Deformation—Packaging-Induced
A
Packing hot parts = secondary deformation source.
Injection Molding PP;deformation;packaging;creep;stacking
Q
PP Injection Part Gloss Deficiency
A
Gloss = replication + mold + grade, three elements.
Injection Molding PP;gloss;replication;polishing;mold temperature
Q
PP Injection Multi-cavity Imbalance
A
For multi-cavity imbalance, first measure filling balance.
Injection Molding PP;multi-cavity;balance;runner;valve gate
Q
PP Injection Part Weld Line Whitening
A
White weld line = cold front + gas and impurity enrichment.
Injection Molding PP;weld line;whitening;venting;overflow well
Q
PP Injection Part Short Material—Poor Venting Type
A
Repeated fixed-point shortage = poor venting—locate with the short shot method.
Injection Molding PP;material shortage;venting;short shot method;gate