POE toughened PP stiffness-toughness balance poor
A
Stiffness-toughness balance requires ternary system and optimized POE particle size
Molding Process POE/PPstiffness-toughness balanceternary compositePOE particle sizenucleating agent
Q
POE/PP dynamic crosslinking crosslinking degree insufficient
A
TPV crosslinking degree insufficient; optimize DCP/TAIC and shear
Molding Process POE/PP TPVdynamic crosslinkingcrosslinking degreeDCPTAIC
Q
POE internal coarse crystallization
A
Coarse crystallization is caused by slow cooling; fast cooling and nucleating agent are key
Molding Process POEcoarse crystallizationspherulite refinementnucleating agentcooling rate
Q
POE toughened PP low-temperature impact insufficient
A
Low-temperature toughening requires lower Tg and stronger interfacial adhesion
Molding Process POE low-temperature tougheningimpact strengthTgPOE-g-MAHEPDM
Q
POE toughened PP impact strength not up to standard
A
The key to POE toughened PP is dispersed phase 0.2-0.5μm and interfacial adhesion
Molding Process POE toughened PPimpact strengthdispersed phase particle sizePOE-g-MAHsilver streak shear band
Q
EPDM surface treatment
A
Surface
Molding Process EPDMsurface
Q
EPDM sponge foaming
A
Sponge
Molding Process EPDMsponge
Q
Ethylene content affects strength
A
Ethylene
Molding Process EPDMethylene
Q
Processing oil selection
A
Oil type
Molding Process EPDMoil
Q
Open mill banding difficulty
A
Banding
Molding Process EPDMbanding