일반적인 플라스틱 재료 문제에 대한 실질적인 답변

1506 질문
Q
PET Bottle Improper Mold Temperature
A
Mold temperature 10~15℃ is the standard window.
Molds & Tooling PET; bottle blowing; mold temperature; bottle sticking; chiller
Q
PET Preform Surface Flow Marks
A
Flow marks = melt front.
Molds & Tooling PET; preform; flow mark; hot runner; speed
Q
PET Preform Weld Line
A
Preform weld line = weak band in blowing.
Molds & Tooling PET; preform; weld line; venting; hot runner
Q
PET Heat-Resistant Bottle (Hot Filling) Deformation
A
Hot filling = special heat-resistant process; ordinary bottles cannot be substituted.
Molds & Tooling PET; hot filling; heat setting; shrinkage; heat resistance
Q
PET Preform Flash
A
Flash = clamping and pressure.
Molds & Tooling PET; preform; flash; clamping; holding pressure
Q
PET Preform Stringing
A
Stringing = gate temperature and timing.
Molds & Tooling PET; preform; stringing; hot runner; valve pin
Q
PET Bottle Single Cavity Abnormality
A
Single cavity abnormality = the water channel or air channel of that cavity; do not touch the global parameters.
Molds & Tooling PET; bottle blowing; mold cavity; cooling water channel; mold temperature