일반적인 플라스틱 재료 문제에 대한 실질적인 답변

2239 질문
Q
LDPE Film Width Deviation
A
Width stability = bubble stability + accurate deviation correction.
Extrusion & Post LDPE; film; width deviation; lay-flat width; deviation correction
Q
LDPE Film Slip Agent Blooming
A
Blooming = excessive additive precipitation.
Extrusion & Post LDPE; film; blooming; slip agent; precipitation
Q
Fast Pressure Differential Rise of LDPE Extrusion Filter Screen
A
Fast pressure differential rise = dual sources of gel + impurities.
Extrusion & Post LDPE; extrusion; filter screen; gel; regrind
Q
LDPE Film Winding Edge Wandering
A
Edge wandering = joint action of tension + thin-thick edges.
Extrusion & Post LDPE; film; winding; edge wandering; tension
Q
Burnt Material at LDPE Extrusion Die Head
A
Burnt material = dead-spot stagnation degradation.
Extrusion & Post LDPE; extrusion; burnt material; die head dead spot; degradation
Q
Unstable Frost Line in LDPE Blown Film
A
The frost line is the thermometer of the blown film process.
Extrusion & Post LDPE; blown film; frost line; air ring; crystallization
Q
Poor Printing Adhesion of LDPE Film
A
Printing adhesion = dyne value + aging.
Extrusion & Post LDPE; film; printing; corona; dyne value
Q
LDPE '2079851475616104452 Mold Sticking
A
Soft material demolding = draft angle + polishing + ejection area.
Extrusion & Post LDPE; '2079851475616104452; mold sticking; draft angle; ejection
Q
LDPE Extrusion Coating Pinholes
A
Pinhole = check three: film rupture + substrate contamination + thin layer.
Extrusion & Post LDPE; extrusion coating; pinhole; coating; substrate
Q
LDPE Extrusion Coating Neck-in
A
Neck-in = elastic shrinkage; adjust oppositely to lowering temperature and increasing speed.
Extrusion & Post LDPE; extrusion coating; neck-in; Neck-in; air gap