일반적인 플라스틱 재료 문제에 대한 실질적인 답변

2239 질문
Q
Head pressure fluctuation of linear low-density polyethylene extruder
Q
Haul-off speed mismatch of linear low-density polyethylene extruded products
A
Haul-off speed mismatch needs to be solved by precisely adjusting haul-off parameters and ensuring haul-off stability.
Extrusion & Post haul-off speedspeed matchinghaul-off slippingclamping forcehaul-off control
Q
Excessive shrinkage of linear low-density polyethylene extruded products
Q
Poor printability of linear low-density polyethylene film
Q
Longitudinal retraction rate of linear low-density polyethylene pipes exceeding standard
Q
Unstable output/surging in the linear low-density polyethylene extrusion process
A
Unstable output is caused by unstable solid conveying; barrel temperature and the feeding system need to be optimized.
Extrusion & Post unstable outputsurgingsolid conveyinghopper bridgingscrew speed
Q
Dimensional fluctuation of linear low-density polyethylene extruded products
A
Dimensional fluctuation is caused by unstable extrusion or haul-off; all process parameters need to be systematically stabilized.
Extrusion & Post dimensional fluctuationscrew speedhaul-off speedtemperature stabilityuniform feeding
Q
Cyclic pressure fatigue failure of linear low-density polyethylene PPR pipes
Q
Thermal aging performance of linear low-density polyethylene PPR pipes not meeting standards
Q
Melt flow rate mismatch of raw material for linear low-density polyethylene extrusion
A
MFR mismatch needs to be solved by selecting suitable grades and adjusting temperature parameters.
Extrusion & Post melt flow rategrade selectionextrusion gradeprocess adjustmentbatch testing
이전 1 ... 43 44 45 46 47 48 49 ... 224 다음