메뉴
재료 기계
인사이트
기사 동영상 문제 및 해결책
About
Chembull 소개 미디어 파트너
문의하기
언어
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어

문제 및 해결책

일반적인 플라스틱 재료 문제에 대한 실질적인 답변

1343 질문
Q
Insufficient strength of linear low-density polyethylene film
Q
Insufficient heat seal strength of linear low-density polyethylene film
A
Insufficient heat seal strength is caused by improper temperature, pressure or time settings; heat seal process parameters need to be optimized.
Material Analysis heat seal strengthheat seal temperatureheat seal pressurefilm thicknessheat seal material
Q
Non-glossy surface of linear low-density polyethylene extruded products
Q
Linear low-density polyethylene PPR pipe welding joint leakage
Q
Mechanical properties of low density polyethylene extruded products not up to standard
Q
Insufficient strength of low density polyethylene film
Q
Insufficient heat seal strength of low density polyethylene film
A
Insufficient heat seal strength is caused by improper temperature, pressure, or time settings; heat seal process parameters need to be optimized.
Material Analysis heat seal strengthheat seal temperatureheat seal pressurefilm thicknessheat seal material
Q
Dull surface of low density polyethylene extruded products
A
Q
Performance degradation caused by excessive regrind ratio in low density polyethylene
Q
Leakage of low density polyethylene PPR pipe welding joints