일반적인 플라스틱 재료 문제에 대한 실질적인 답변

1343 질문
Q
PU hydrolytic aging
A
Hydrolytic aging is caused by polar groups being sensitive to water; selecting low polarity grade is key
Material Analysis PU hydrolytic aging polar groups anti-hydrolysis stabilizer waterproof coating
Q
Heavy smoke in PU processing
A
Heavy smoke is caused by volatiles evaporation; temperature reduction and exhaust are key
Material Analysis PU processing smoke volatiles exhaust system temperature reduction
Q
Insufficient toughness of PU, brittle fracture
A
Insufficient toughness is caused by low molecular weight and coarse crystallization; selecting high MW is key
Material Analysis PU insufficient toughness molecular weight crosslinking control crystallization refinement
Q
Poor chemical resistance of PU
A
Poor chemical resistance is caused by PU chemical affinity; selecting chemical-resistant grade and coating are key
Material Analysis PU chemical resistance chemical attack slight crosslinking surface coating
Q
Strong odor in PU processing
A
Strong odor is caused by PU decomposition and volatilization; temperature control and ventilation are key
Material Analysis PU processing odor volatiles ventilation and exhaust temperature control
Q
Large creep deformation of PU
A
Large creep is caused by elastomer nature; slight crosslinking and rigid filler are key
Material Analysis PU creep slight crosslinking high molecular weight rigid filler
Q
Insufficient tensile strength of PU
A
Insufficient tensile strength is caused by molecular weight and poor interface; selecting high MW grade is key
Material Analysis PU tensile strength molecular weight coupling agent orientation control
Q
Bubbles in PU elastomer casting
A
PU casting bubbles are caused by insufficient degassing; vacuum degassing is key
Material Analysis PU casting bubbles vacuum degassing casting temperature mixing degassing
Q
Low elongation at break of PU
A
Low elongation at break is caused by low molecular weight and orientation; selecting high MW and reducing orientation are key
Material Analysis PU elongation at break molecular weight orientation control crosslinking degree
Q
PU hardness too high
A
High hardness is caused by crystallization and filler; adjusting cooling and filler are key
Material Analysis PU high hardness crystallinity filler amount plasticizer