إجابات عملية على التحديات الشائعة في مواد البلاستيك

1506 سؤال
Q
Burning from poor venting in PET preform '2079851475616104452
Q
Uneven crystallization white haze of PET injection products
A
PET crystallization behavior is very sensitive to mold temperature; uniform mold temperature is key.
Injection Molding PETuneven crystallizationwhite hazemold temperaturespherulite
Q
Large shrinkage rate fluctuation of PET injection parts
Q
Yellowing and embrittlement of PET injection products
Q
Rough inner wall from barrel wear of PCTG injection machine
Q
Poor plasticization from improper screw rotation speed of PCTG injection machine
A
PCTG screw rotation speed is a plasticizing quality variable.
Injection Molding PCTGscrew rotation speedplasticizing quality
Q
Over-temperature risk of oil temperature machine in PCTG '2079851475616104452
A
PCTG mold temperature control equipment needs to be precise and reliable.
Injection Molding PCTGoil temperature machineover-temperaturemold
Q
Sudden pressure rise alarm in PCTG '2079851475616104452
A
PCTG sudden pressure rise is a runner blockage signal.
Injection Molding PCTGsudden pressure riseblockagealarm
Q
Nozzle blockage in PCTG '2079851475616104452
A
PCTG nozzle freezing requires heat preservation and cleaning.
Injection Molding PCTGnozzle blockageheat preservationinsulation
Q
Deformation from short cycle (insufficient cooling) in PCTG '2079851475616104452