1506 سؤال
Q
Burn Marks Appearing at the Weld Line Position of ABS-type variant Injection-Molded Products
A
This problem needs to be systematically solved from three aspects: material characteristics, process parameters, and mold conditions.
Injection Molding burn markweld line positionABS-type variant'2079851475616104452process optimization
Q
Burn Marks Appearing at the Weld Line Position of ABS variant Injection-Molded Products
Q
Glass Fiber Exposure (Floating Fiber) Appearing on the Surface of Glass Fiber Reinforced polyamide 66 (nylon 66) Products
Q
Glass Fiber Exposure (Floating Fiber) Appearing on the Surface of Glass Fiber Reinforced polyamide 6 (nylon 6) Products
Q
Glass Fiber Exposure (Floating Fiber) Appearing on the Surface of Glass Fiber Reinforced polyamide 56 (bio-based nylon) Products
Q
Glass Fiber Exposure (Floating Fiber) Appearing on the Surface of Glass Fiber Reinforced polyamide 46 (high-temperature nylon) Products
Q
PA46 Processing Temperature as High as 290-330°C
A
PA46 requires ultra-high temperature special equipment
Injection Molding PA46high-temperature equipmentbarrelscrew heat resistance
Q
Glass Fiber Appearing on the Surface of Glass Fiber Reinforced polyamide 410 (bio-based long carbon chain nylon) Products
Q
Glass fiber exposure (flo on the surface of glass fiber reinforced polyamide 12 (long carbon chain nylon) products
A
Q
Glass fiber exposure (floating fiber) on the surface of glass fiber reinforced polyamide (general-purpose nylon) products
A