Q
POM product insert cracking
A
Inserts = preheating + wall thickness.
Molding Process POM;inserts;cracking;preheating
Q
POM product welding problem
A
Welding = precise interface temperature.
Molding Process POM;welding;ultrasonic welding;parameters
Q
POM product static dust attraction
A
Static electricity = a common problem of insulating materials.
Molding Process POM;static electricity;dust attraction;antistatic
Q
POM product stress cracking
A
Cracking = stress + medium.
Molding Process POM;stress cracking;internal stress;medium
Q
POM regrind usage problem
A
POM regrind = the less used the better.
Molding Process POM;regrind;degradation;formaldehyde;thermal history
Q
POM weld line weak strength
A
POM weld lines = racing against crystallization speed.
Molding Process POM;weld line;crystallization;melt temperature;gate