Injection Molding 3 Aufrufe

ABS cushion fluctuation causing alternating short shot and flash

Problembeschreibung
Under the same process, short shots and flash of the product appear alternately, with large weight fluctuations.
Ursachenanalyse
The check ring is worn or stuck, causing the melt to flow back during injection, and the actual shot volume is unstable; the cushion fluctuates large and small.
Lösung
①Detect the cushion fluctuation (30 consecutive shots); ②disassemble and inspect the check ring wear and replace it; ③clean foreign matter at the screw head; ④stabilize the back pressure and speed.
Wichtigste Erkenntnis
When short shots and flash appear alternately, suspect the check ring first.
ABS;check ring;cushion;metering instability;backflow