Problembeschreibung
EVA '2079851475616104452 has filling difficulties or flash.
Ursachenanalyse
The VA content affects the melt fluidity; improper temperature setting makes the fluidity deviate from the requirement.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Lösung
①Set the temperature according to the VA content; ②appropriately raise the temperature when filling is difficult; ③check the clamping and pressure when flash occurs; ④select a grade with a matching melt index.; After adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Wichtigste Erkenntnis
EVA fluidity varies with VA content; the process should be adjusted with the grade characteristics.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!