Injection Molding 3 Aufrufe

HDPE '2079851475616104452 weld lines

Problembeschreibung
The weld lines of HDPE products are obvious and weak.
Ursachenanalyse
Fast crystallization; when the front confluence temperature is insufficient, the bond is weak; more obvious with poor venting.
Lösung
①Increase melt temperature and speed; ②vent at the confluence; ③adjust the gate position; ④increase the mold temperature.
Wichtigste Erkenntnis
Weld lines: grab temperature, keep venting.
HDPE; '2079851475616104452; weld line; venting; melt temperature