Processing Machinery 5 Aufrufe

HDPE barrel temperature zoning

Problembeschreibung
HDPE plasticization is uneven with entrained unmelted particles
Ursachenanalyse
The barrel temperature gradient is unreasonable, and melting in the compression section is insufficient; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Lösung
Barrel gradient: rear section 180℃, middle section 210℃, front section 230℃; back pressure 0.3-0.8MPa; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
HDPE temperature gradient rises gently to ensure plasticization; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar future problems
HDPEbarrel temperatureplasticizationback pressure