LDPE Film Weak Edge (Slitting Edge Burst)
Problembeschreibung
After slitting, the film edge is serrated and tears easily and extends.
Ursachenanalyse
Blunted cutters and excessive slitting tension; when the film itself has high MD strength and weak TD (splitty), edge cracking is easier.
Lösung
①Replace/sharpen cutters; ②adjust slitting tension; ③evaluate longitudinal-transverse stretch balance; ④adjust blow-up ratio and draw ratio.
Wichtigste Erkenntnis
Edge burst = cutter + tension + orientation balance.