LDPE Insufficient Longitudinal Strength
Problembeschreibung
LDPE film has low longitudinal tensile strength
Ursachenanalyse
Insufficient longitudinal draw ratio causes insufficient molecular orientation; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Lösung
Increase the haul-off ratio; match the blow-up ratio; select high-strength grades; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate the effective measure
Wichtigste Erkenntnis
Longitudinal strength relies on draw orientation design; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!