LLDPE film haze process optimization
Problembeschreibung
Attempts to reduce LLDPE film haze through process means have limited effect.
Ursachenanalyse
Fast cooling can reduce crystallite size and lower haze; but the haze lower limit determined by the LLDPE molecular structure is higher than LDPE.; During on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience.
Lösung
①Strong cold air rapid cooling; ②appropriately lower the frost line; ③raise melt temperature to improve plasticization; ④switch to mLLDPE for demanding occasions.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Wichtigste Erkenntnis
Process can optimize but hardly breaks through the material limit; transparent applications should directly select metallocene grades.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!