LLDPE melt temperature 200-260℃

Problembeschreibung
Low melt temperature causes insufficient filling; high melt temperature causes product discoloration and degradation, and prolongs the cycle.
Ursachenanalyse
LLDPE's short branched chain structure gives good melt fluidity, with a processing window of 200-260℃; too high a temperature gives better fluidity but slower cooling, a longer cycle and possible degradation.
Lösung
①'2079851475616104452 melt temperature 200-260℃ adjusted by product; ②film extrusion optimized by grade; ③beware of thermal oxidative degradation above 280℃; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Wichtigste Erkenntnis
LLDPE's wide temperature window reflects process friendliness; but high-temperature residence also causes degradation, and leniency does not mean no boundary; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
LLDPE; melt temperature; 200-260℃; 280℃; degradation