Injection Molding 5 Aufrufe

LLDPE '2079851475616104452 temperature management

Problembeschreibung
LLDPE '2079851475616104452 discolors at slightly high temperature; the temperature window is narrower than LDPE.
Ursachenanalyse
LLDPE '2079851475616104452 temperature 200-260℃ is close to LDPE, but the narrow MWD makes viscosity more temperature-sensitive; slightly high temperature may cause degradation; precision parts need stricter temperature control.
Lösung
①Melt temperature 200-260℃ adjusted by grade; ②precision parts temperature control ±5℃; ③immediately lower the temperature and purge when discoloration occurs; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Wichtigste Erkenntnis
LLDPE '2079851475616104452 temperature management is stricter than LDPE; the viscosity sensitivity of narrow MWD requires finer temperature control; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
LLDPE; '2079851475616104452 temperature; 200-260℃; ±5℃; precision