Processing Machinery
2 Aufrufe
LLDPE sharkskin
Problembeschreibung
LLDPE film sharkskin is more severe than LDPE
Ursachenanalyse
LLDPE narrow molecular weight distribution has poor shear-thinning ability and is highly sensitive to melt fracture; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Lösung
Large die gap; increase melt temperature; add PPA aid; reduce speed; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Wichtigste Erkenntnis
LLDPE sharkskin requires both equipment and additive measures; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
War das hilfreich?
0 Personen fanden dies hilfreich