Stress cracking of PA6 injection molded products
Problembeschreibung
Cracking after contact with grease and solvents.
Ursachenanalyse
PA6 is sensitive to certain chemicals, internal stress + medium induces cracking; high-stress areas crack first; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience.
Lösung
①Reduce internal stress; ②conduct medium compatibility/immersion verification before mass production; ③fillet design; ④optimize assembly design to avoid excessive interference; ⑤perform annealing treatment when necessary to eliminate residual stress.
Wichtigste Erkenntnis
PA6 cracking='stress + medium': reducing stress and avoiding the medium on both fronts; nylon internal stress management must be addressed from both process and structure; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!