Material Analysis
10 Aufrufe
rPET Bottle Black Speck Impurities
Problembeschreibung
Tiny dark impurity dots are visible on the 100% rPET bottle wall, and high-end packaging receives complaints.
Ursachenanalyse
Recycled PET raw material contains trace residual impurities from previous use; the filtration precision of the regeneration process is limited, and impurities are conspicuous on transparent bottle walls.
Lösung
①Improve the filtration precision of recycled material; ②agree with the customer on impurity acceptance standards (e.g. quantity upper limit for <0.5mm); ③control the rPET ratio for high-transparency applications; ④strengthen incoming material inspection.
Wichtigste Erkenntnis
rPET impurities = the upper limit of the regeneration process; standards agreed in advance.