Injection Molding 5 Aufrufe

PET injection machine selection

Problembeschreibung
Using an ordinary '2079851475616104452 machine to process PET, the temperature control is unstable and product quality fluctuates greatly
Ursachenanalyse
PET has a high melting point and a short stability time after the melting point, requiring an injection system with many temperature control zones and little self-friction heat generation; when the shot weight is less than 2/3 of the machine's injection capacity, the melt is retained too long and degrades
Lösung
①Select a PET-specific plasticizing system with many temperature control zones; ②the actual weight of the product including the runner is not less than 2/3 of the machine's injection capacity; ③calculate the clamping force at 6300 t/m² or above
Wichtigste Erkenntnis
PET has specific requirements for the '2079851475616104452 machine; the number of temperature control zones and the shot weight ratio are the two major verification items for equipment matching; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PET;injection machine selection;temperature control zones;shot weight;clamping force