Processing Machinery
2 Aufrufe
PET die opening buildup
Problembeschreibung
Buildup at the PET die lip gradually increases, and the sheet carries streaks
Ursachenanalyse
Low-molecular substances in the melt precipitate and accumulate at the die opening, periodically falling off to form streaks and impurities; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Lösung
Regularly clean the die opening; lower the melt temperature to reduce precipitation; verify by changing the raw material grade; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Wichtigste Erkenntnis
Die opening buildup is the accumulation of precipitates; cleaning plus temperature management; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
War das hilfreich?
0 Personen fanden dies hilfreich