Thermoforming
3 Aufrufe
PP '2079851475616104458 Webbing
Problembeschreibung
Material piles up and wrinkles at corners during PP/TPO sheet '2079851475616104458.
Ursachenanalyse
Sheet overheating with excessive sag, surplus area, vacuum applied too late; olefin materials with low melt strength pile up more easily.
Lösung
①Lower heating temperature or shorten heating time; ②use pre-blow bubble (billow) pre-stretching; ③cut the sheet smaller; ④enlarge mold fillets.
Wichtigste Erkenntnis
For olefin sheet '2079851475616104458, make good use of pre-blow bubbles to prevent webbing.