Processing Machinery 2 Aufrufe

PPO Cushion and Metering Stroke

Problembeschreibung
【Problem Phenomenon】PPO metering is unstable, and product weight and dimensions fluctuate
Ursachenanalyse
GTX974 data gives metering stroke 0.5-3.5D and residual cushion 3-6mm (depending on metering stroke and screw diameter); improper cushion makes pressure transmission unstable
Lösung
Set metering stroke at 0.5-3.5D; keep residual cushion at 3-6mm; for weight fluctuation, check cushion and non-return ring first; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Wichtigste Erkenntnis
PPO cushion 3-6mm ensures pressure transmission, metering stroke 0.5-3.5D is the boundary; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence