Problembeschreibung
[Problem Phenomenon] Exposed fibers and rough surface on PPO+40% glass fiber products
Ursachenanalyse
When glass fiber content is high, fibers are enriched on the surface with melt flow; low melt and mold temperatures and slow injection speed aggravate floating fiber; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Lösung
Raise melt and mold temperatures to improve fiber encapsulation; increase injection speed to embed fibers; optimize gates to reduce orientation concentration; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
Floating fiber of PPO high-fiber grades is suppressed by temperature and injection speed, with gates cooperating for homogenization; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!