PP Black Speck Thermal Decomposition

Problembeschreibung
PP black specks from thermal decomposition, melt over 300°C or residence too long, temperature management.
Ursachenanalyse
PP black specks from thermal decomposition; melt temperature over 300°C; residence time too long; screw wear; incomplete purging; material degradation.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Lösung
①Melt temperature ≤300°C; ②shorten residence time; ③screw inspection; ④purging specifications; ⑤degradation monitoring.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
Temperature and residence are the main causes of PP black specks; equipment and purging are equally important; monitoring prevents degradation.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PP;black speck;thermal decomposition;300°C;residence;purging