HIPS Sheet Surface Gel Particles
Problembeschreibung
Unplasticized particles appear on the sheet surface.
Ursachenanalyse
Poor plasticization or insufficient filtration allows unmelted particles to enter the sheet; raw material impurities are also a source.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Lösung
①Optimize plasticization temperature; ②strengthen filtration; ③clean die head dead corners; ④strengthen raw material inspection.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
Gel particle control relies on plasticization and filtration; high-requirement sheets use finer screens.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!