Menü
Materialien Maschinen
Einblicke
Artikel Videos Problem & Lösung
About
Über Chembull Medienpartner
Kontaktieren Sie uns
Sprache
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Zurück zu Problem & Lösung
Processing Machinery 2 Aufrufe

PVDF Product Weld Line

Problembeschreibung
Low weld line strength.
Ursachenanalyse
Low melt front temperature and poor fusion; PVDF crystallizes quickly and the melt front cools significantly.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; This mechanism has been repeatedly verified by industry materials, and it should be confirmed first during troubleshooting
Lösung
①Increase melt and mold temperatures; ②optimize gate position; ③increase confluence speed; ④set an overflow well.; After adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
Weld lines are managed by temperature and gate.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; Include this case in the defect archive as a reference for troubleshooting similar problems in the future
PVDF;weld line;temperature;gate;confluence;overflow well

War das hilfreich?

0 Personen fanden dies hilfreich

ChemAI