Molding Process
6 Aufrufe
Processing Temperature Too Low Causing Poor Plasticization
Problembeschreibung
Below 160C, plasticization is insufficient and the surface is rough
Ursachenanalyse
Low temperature, not fully melted, insufficient plasticization
Lösung
Raise to the reasonable range of 160-190C
Wichtigste Erkenntnis
The processing temperature window determines plasticization
War das hilfreich?
0 Personen fanden dies hilfreich