EAA surface blooming
Problembeschreibung
EAA product surface precipitates white frost-like low molecular substances affecting appearance
Ursachenanalyse
Low molecular components in EAA migrate to the surface and precipitate during storage; lubricant or plasticizer supersaturated and precipitating
Lösung
1) Select high molecular weight EAA to reduce low molecular substances; 2) Reduce lubricant addition to a reasonable level; 3) Clean the product surface and then test to identify the source
Wichtigste Erkenntnis
Blooming is caused by low molecular migration and precipitation; selecting a high molecular weight grade is fundamental