Injection Molding
4 Aufrufe
Periodic EAA surface ripples
Problembeschreibung
Periodic ripples on the EAA product surface with spacing of 5-15mm
Ursachenanalyse
Injection speed fluctuating periodically; hydraulic system unstable; screw speed unstable
Lösung
1) Overhaul the injection system to stabilize pressure and speed; 2) Use servo motor drive instead of hydraulic drive; 3) PID control to stabilize injection parameters
Wichtigste Erkenntnis
Ripples are caused by unstable injection; equipment overhaul and PID control are key
War das hilfreich?
0 Personen fanden dies hilfreich