EEA Flame Retardancy Not Up to Standard
Problembeschreibung
EEA product flame retardant rating is V-2 or not rated
Ursachenanalyse
Insufficient flame retardant addition; poor compatibility between flame retardant and EEA, uneven dispersion; flame retardant decomposes and fails during processing
Lösung
1) Increase flame retardant to the recommended dosage of 15-25wt%; 2) Select EEA-specific flame retardant to ensure compatibility; 3) Use flame retardant masterbatch method to ensure uniform dispersion
Wichtigste Erkenntnis
Flame retardancy not up to standard is caused by insufficient dosage and poor compatibility; increasing dosage and dedicated flame retardant are key