Processing Machinery
3 Aufrufe
EEA Insufficient Compounding
Problembeschreibung
After blending EEA with fillers/additives, dispersion is uneven with local agglomeration
Ursachenanalyse
Insufficient screw mixing section length; insufficient number of kneading blocks; improper feeding method, additives not in full contact with EEA
Lösung
1) Increase screw mixing section length to 3-4D; 2) Increase the number of kneading blocks; 3) Add additives later through the side feeding port to increase mixing time
Wichtigste Erkenntnis
Insufficient compounding is caused by improper screw design; increasing the mixing section is key