EEA Low Flexural Modulus

Problembeschreibung
EEA product flexural modulus is 20% lower than the design value
Ursachenanalyse
EEA soft, low modulus; insufficient filler addition or poor interface, no reinforcing effect; crystallinity low
Lösung
1) Add 10-15wt% rigid filler to increase modulus; 2) Nucleating agent to increase crystallinity; 3) Select high-modulus grades
Wichtigste Erkenntnis
Low flexural modulus is caused by material softness and insufficient filler; adding rigid filler is key
EEA flexural modulus rigid filler nucleating agent crystallinity