Processing Machinery 3 Aufrufe

EEA Internal Black Speck Carbonization

Problembeschreibung
0.1-0.5mm black speck carbonized matter appears inside EEA products
Ursachenanalyse
EEA carbonized by prolonged heating in barrel dead zones; carbon deposits on the screw head; raw material impurities
Lösung
1) Lower processing temperature to reduce carbonization; 2) Regularly clean the screw and barrel; 3) Filter raw material to remove impurities
Wichtigste Erkenntnis
Black specks are caused by thermal carbonization and carbon deposits; lowering temperature and regular cleaning are key
EEA internal black specks thermal carbonization screw cleaning temperature control