Material Analysis 10 Aufrufe

EMA hardness too high

Problembeschreibung
EMA product Shore hardness 5-10 degrees higher than target, feeling hard
Ursachenanalyse
EMA crystallinity too high increasing rigidity; too much filler added; cooling too fast with incomplete crystallization but rigidity frozen
Lösung
1) Reduce cooling rate to complete crystallization and reduce hard feel; 2) Reduce filler addition; 3) Add plasticizer 0.5wt% to lower hardness
Wichtigste Erkenntnis
High hardness is caused by crystallization and filler; adjusting cooling and filler is key
EMA hardness too high crystallinity filler amount plasticizer