Menü
Materialien Maschinen
Einblicke
Artikel Videos Problem & Lösung
About
Über Chembull Medienpartner
Kontaktieren Sie uns
Sprache
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Zurück zu Problem & Lösung
Molding Process 6 Aufrufe

EMA hardness too low

Problembeschreibung
EMA product Shore hardness 5-10 degrees lower than target, feeling soft
Ursachenanalyse
EMA soft nature with low hardness; too much plasticizer or softener added; crystallinity too low
Lösung
1) Add rigid filler 5-10wt% to increase hardness; 2) Reduce plasticizer dosage; 3) Increase cooling rate to increase crystallinity
Wichtigste Erkenntnis
Low hardness is caused by material softness and excessive plasticization; adding filler is key
EMA hardness too low rigid filler plasticizer crystallization control

War das hilfreich?

0 Personen fanden dies hilfreich

ChemAI