Processing Machinery 3 Aufrufe

EVOH Material Changeover Residue

Problembeschreibung
After EVOH material changeover, the first 5-10 products contain previous material residue with color difference and property deviation
Ursachenanalyse
Large amount of previous material residue in barrel and screw; cleaning incomplete with residue in dead zones; purging compound amount insufficient
Lösung
1) Increase purging compound amount to 2-3 times barrel capacity; 2) Increase rotation speed and temperature during cleaning to accelerate removal; 3) Disassemble screw to thoroughly clean dead zones
Wichtigste Erkenntnis
Changeover residue is caused by incomplete cleaning; thorough cleaning and disassembly are key
EVOHchangeover residuepurging compoundscrew disassemblydead zone cleaning