EVOH Hardness Too High

Problembeschreibung
EVOH product Shore hardness 5-10 degrees above target, hard to the touch
Ursachenanalyse
EVOH crystallinity too high, rigidity increased; filler added too much; cooling too fast, crystallization imperfect but rigidity frozen in
Lösung
1) Reduce cooling rate to perfect crystallization and reduce hard feel; 2) Reduce filler addition; 3) Add plasticizer 0.5wt% to lower hardness
Wichtigste Erkenntnis
High hardness is caused by crystallization and filler; adjusting cooling and filler is key