EVOH Hardness Too Low
Problembeschreibung
EVOH product Shore hardness 5-10 degrees below target, soft to the touch
Ursachenanalyse
EVOH soft nature, hardness low; plasticizer or softener added too much; crystallinity too low
Lösung
1) Add rigid filler 5-10wt% to increase hardness; 2) Reduce plasticizer amount; 3) Increase cooling rate to raise crystallinity
Wichtigste Erkenntnis
Low hardness is caused by material softness and excessive plasticization; adding filler is key