Material Analysis 10 Aufrufe

EVOH Hydrolytic Aging

Problembeschreibung
EVOH products in hot-humid environment show mechanical decline >25%
Ursachenanalyse
EVOH contains polar groups that hydrolyze and break chains under hot-humid conditions; ester bonds/amide bonds etc. are water-sensitive
Lösung
1) Select low-polarity-content grade to reduce hydrolysis tendency; 2) Add anti-hydrolysis stabilizer; 3) Coat product surface with waterproof layer
Wichtigste Erkenntnis
Hydrolytic aging is caused by water-sensitive polar groups; selecting low-polarity grade is key