Injection Molding 2 Aufrufe

Severe internal stress concentration of PU

Problembeschreibung
Internal stress of PU products >15MPa, causing cracking during storage
Ursachenanalyse
Injection speed too fast, large orientation stress; uneven cooling freezing thermal stress; improper gate position, concentrated flow orientation
Lösung
1) Reduce injection speed to reduce orientation; 2) Uniform mold temperature to reduce thermal stress; 3) Anneal at 80°C/4h to release stress; 4) Optimize gate position
Wichtigste Erkenntnis
Internal stress is caused by fast injection and uneven cooling; speed reduction, uniform cooling and annealing are key
PU internal stress orientation stress annealing treatment uniform cooling