Insufficient PU mixing
Problembeschreibung
After blending PU with fillers/additives, dispersion uneven, local agglomeration
Ursachenanalyse
Screw mixing section length insufficient; insufficient number of kneading blocks; improper feeding method, additives not fully in contact with PU
Lösung
1) Increase screw mixing section length to 3-4D; 2) Increase number of kneading blocks; 3) Add additives after the side feed port to increase mixing time
Wichtigste Erkenntnis
Insufficient mixing is caused by improper screw design; increasing the mixing section is key