Insufficient PVA toughness, brittle fracture
Problembeschreibung
PVA product elongation at break <50%, brittle fracture without yielding
Ursachenanalyse
PVA molecular weight on the low side, insufficient toughness base; excessive crosslinking losing toughness; coarse crystallization, increased brittleness
Lösung
1) Select high molecular weight PVA to improve toughness; 2) Control crosslinking degree to avoid excess; 3) Nucleating agent to refine crystallization and improve toughness
Wichtigste Erkenntnis
Insufficient toughness is caused by low molecular weight and coarse crystallization; selecting high MW is the key