Processing Machinery 3 Aufrufe

PVA internal black speck carbonization

Problembeschreibung
PVA product interior shows 0.1-0.5mm black specks of carbonized material
Ursachenanalyse
PVA heated for a long time in barrel dead zones and carbonized; carbon deposit at the screw head; raw material impurities
Lösung
1) Lower processing temperature to reduce carbonization; 2) Regularly clean the screw and barrel; 3) Filter raw material to remove impurities
Wichtigste Erkenntnis
Black specks are caused by thermal carbonization and carbon deposit; temperature reduction and regular cleaning are the key
PVAinternal black speckthermal carbonizationscrew cleaningtemperature control