Product shows multiple defects (silver streaks, burnt, short shot, etc.)

Problembeschreibung
Product shows multiple defects (silver streaks, burnt, short shot, etc.), related to unreasonable barrel temperature settings
Ursachenanalyse
Barrel zone temperature settings unreasonable, not set according to the cellulose acetate butyrate recommended range 170-230°C Large temperature fluctuation, thermocouple or heater band failure Front zone temperature too high, rear zone temperature on the low side, uneven melt Unreasonable temperature gradient setting causing poor plasticization Temperature control system slow response, large deviation between actual temperature and setpoint
Lösung
Reasonably set each zone temperature according to the 170-230°C range Check and maintain the temperature control system to ensure stability Reasonably set temperature gradient increasing from rear zone → front zone Appropriately lower front zone temperature to prevent degradation Calibrate the temperature control system to reduce deviation
Wichtigste Erkenntnis
Barrel temperature needs to be stably set according to the material recommended range