Injection Molding 2 Aufrufe

CEF injection flow marks

Problembeschreibung
Radial flow marks centered on the gate appear on the surface of the CEF injection molded part
Ursachenanalyse
The injection speed is too fast, causing the melt front to be unstable; the mold temperature is too low <30°C and the front cools rapidly to form marks
Lösung
1) Adopt multi-stage injection speed slow-fast-slow to control the stability of the front; 2) Increase the mold temperature to 40-50°C to delay the cooling of the front; 3) Stabilize the injection pressure to avoid fluctuations; 4) Increase the gate area to reduce sudden pressure changes at the gate
Wichtigste Erkenntnis
Flow marks are caused by unstable injection front and rapid cooling; multi-stage injection and high mold temperature are the key