Molding Process 6 Aufrufe

Poor Thickness Uniformity of CMC Extruded Film

Problembeschreibung
Transverse thickness deviation of CMC extruded film is ±15%, exceeding the ±5% industry standard
Ursachenanalyse
Unreasonable die flow channel design causes uneven melt flow in the wide die; CMC melt elasticity is large and die swell is uneven; air ring cooling is uneven
Lösung
1)Adopt coat-hanger die design to ensure uniform transverse flow; 2)Fine-tune die gap ±0.02mm; 3)Optimize air ring air volume and angle for uniform cooling; 4)Add a small amount of low-elasticity resin to reduce swell difference
Wichtigste Erkenntnis
Film thickness uniformity needs coordinated optimization from three aspects: die design, gap adjustment and cooling
CMC filmthickness uniformitydie designdie swellair ring cooling